Product Description
Product name : Vietnam natural rubber SVR 3L
SVR3L is produced from field latex.It is light color with excellent tensile.It is widely used in performance tyres, industrial rollers and other applications requiring high quality.And its adhesion performance is very good.Sometimes SVR 3L can replace TSR5 grade rubbers.
Handling Precautions:
Direct exposure to sunlight and humidity may cause discoloration or quality deterioration. Keep the product away from direct sunlight,humidity and impurities,and store in a cool place.
Specification Sheets:
Property
|
Limits SVR3L
(TCVN3679:2004)
|
Standard
(Test method)
|
Ditretained on 45μaperture),
(%wt)Max
|
0.03
|
TCVN 6089:2004
(ISO 249:1995)
|
Ash Content, (%wt)Max
|
0.50
|
TCVN 6087:2004
(ISO 247:1990)
|
Volatile matter, (%wt)Max
|
0.80
|
TCVN 6088:2004
(ISO 248:1991)
|
Nitrogen, (%wt)Max
|
0.60
|
TCVN 6092-2:2004
(ISO 2007:1991)
|
Initial Wallance Plasticity
(Po)Min
|
35
|
TCVN 6092-1:2004
(ISO 2930:1995)
|
PRI(p30/ Po)×100Min
|
60
|
TCVN 6089:2004
(ISO 249:1995)
|
Lovibond colour Max
|
6
|
TCVN 6093:2004
(ISO 4660:1999)
|
Mooney Viscosity
ML(1’+4’)100°C
|
-
|
TCVN 6090:2004
(ISO 289-1:1994)
|
Rheometric Cure(160°C,1° are 100rpm,ACS1)
|
|
TCVN 6094:2004
(ISO 3417:1991)
|
-Torque Min,(dNm)
|
-
|
|
- Torque Max,(dNm)
|
-
|
|
-Scorch Time T2(m:s)
|
-
|
|
-Optimum Cure Time t90, (m:s)
|
-
|
|
Transportation:
Packing:
|
33.3kgs/bale
|
Loading:
|
20MT/20FCL
|
Delivery time:
|
Within 20 days after receiving your deposite
|
|
Product Image
Img 1
Send Inquiry to this Member
Related Products of this Company
This member assumes full responsibility for the content of this listing. DIYTrade accepts no responsibility whatsoever in respect of such content.
To report fraudulent or illegal content, please
click here.
China Suppliers Quick Searching:
,