Model: | 901040 |
---|---|
Brand: | lianhuan silicone |
Origin: | Made In China |
Category: | Chemicals / Rubber Materials |
Label: | Eco-friendly silicon , Silicone Textile sil , textile printing sil |
Price: |
US $12.5
/ kg
|
Min. Order: | 1 kg |
Last Online:02 Aug, 2017 |
Silicone ink Appliation :
Suitable for most natural and synthetic fabrics, including elastic fabrics for these garments:
·Jerseys
·Hats & caps
·Sweaters
·Jackets
·Gloves
·Sleepwear
·Pants & shorts
·Bathing suits
·Undergarments
·Uniforms
·Shirts
·Sweatshirts
Silicone Ink features:
·Good hand feel: Soft, non-sticky handle with no blocking problem upon folding
·Excellent durability: Wash- and weather-resistance
·Color fastness: No color migration, even between red and white
·Improved fashion appearance: Semi-gloss finish with no creasing
·High elongation: Suitable for fabric with Lycra content
·Fast cure: Skin cures in 3 to 6 seconds at skin temperatures between 100-130°C
·Operation-friendly: Suitable viscosity and thixotropy for manual screen printing
·Easily pigmented: A base gel / catalyst system of less than 10 percent
·Environmentally sound: Does not contain organotin, phthalate, formaldehyde, PVC or solvent
·Reduced total cost of use: Lower process time and better coverage
·Low shrinkage(<0.1%)
·Excellent performance of anti-slip
·Good skid-proof effect and high adhesive strength
·Wearproof, wash-resistant, high temperature resistant
·Non-toxic and odorless, food grade silicone
·High transparency and good tear-strength
·Wearproof, washable, high temperature resistance
·Three-dimensional level
·
Silicone Ink Datasheet :
Model |
901040 |
903540 |
Appearance |
Transparent |
Transparent |
Hardness(shore A) |
35±2 |
42±2 |
Mix ratio(A:B) |
10:1 |
10:1 |
Viscosity(mPa.s) |
60000~100000 |
300000~380000 |
Tensile strength(Mpa) |
4.6 |
4.8 |
Tear-strength(KN/m) |
20±2 |
22±2 |
Elongation(%) |
450 |
420 |
Pot life/working time(25degree) |
2-3 hours |
2-3 hours |
curing time(125degree) |
30~50 seconds |
30~50 seconds |
(ps: the hardness and viscosity is adjustable)
Silicone Ink Prepare Methods:
Mixed Color master batch: Using it when needing various colors.
For ink to be yellow: first change base A part to white color (10%) white pigment in. then mixed with yellow color paste1% to colors!
Same process as for ink to blue and Red ink!
For ink to be black : add 5% of black color paste to base A part mixed well.For ink to be grey: add 3% of black color paste and 5% of white color paste to base A part mixed well
Silicone Ink Mix process :
1. Mixed 10% CATATLYST curing agent B Part into small amount of silicone ink A Part(90%).
2. The curing agent should be mixed very well, Otherwise,some parts won’t be cured.
3. could use thinner for decrease the viscosity,over 15% of thinner, the abrasiveness, durability and adhesion force will be reduce. There tested before production is required.
Silicone Ink Drying Methods:
1. According to different thickness of silicone ink, the curing time is different. Normal situation for mixing Part A: Part B =10:1 curing time is 50seconds with the temperature of 150degree (polyaddition process).
2. When the room temperature is above 25degree (humidity 50%), room temperature cure can be carried out under summer condition
3.Color master batch: Using it when needing various colors.
Quality Inspection
More details, please contact MS Nancy Xie
Phone: 0086-13699849627
Skype: nancyxie2007
Website: www (dot) lhsilicone (dot) com
Payment Terms: | TT |
---|---|