Min. Order: | 1000 kg |
Last Online:04 Dec, 2015 |
Fireproof Ceramic Fiber Cloth Manufacturer
We are a Chinese weaving mill of fiberglass fabric, ceramic fiber textile (yarn, cloth,tape, rope).
Our ceramic fiber cloth, fiberglass backed aluminium foil and colored fiberglass fabric are widely used in fire shutter doors, coiling doors, smoke curtains and other fire safety and blinds application.
We have 260 sets of rapier looms, and 6 sets of ceramic fiber cloth production lines.
We also have 4 sets of aluminium foil laminating machines, and one set silicon ruber coating machine.
The ceramic fiber products we suppy includes ceramic fiber ropes, braids, cloth, tapes & sleeving. These ceramic fiber textiles are made from alumina-silica ceramic fiber (47% Alumina, 53% silica), free of asbestos & free silica. These ceramic fiber textile materials can be used in different industrial applications in temperatures up to 2300F (1260C), have excellent chemical stability and strong resistance to thermal shock and corrosion attack. Exceptions are hydrofluoric and phosphoric acids and concentrated alkalies. These ceramic fiber textiles also resist oxidation and reduction.
-Gasket and wrapping material
-Pipe hanger insulation
-Welding curtains and blankets
-Fuel line insulation
-Furnaces heat zone separators
-Exhaust hood curtains
-Cable and wire insulation
-Induction heating furnace coil insulation
-infrared radiating diffusers
-High pressure steam portable flange covers
ITEM | Fireproof Ceramic Fiber Cloth Manufacturer |
MATERIAL | alumina-silica ceramic fiber |
tHICKNESS | 2MM, 3MM, 5MM |
WIDTH | 1000-1250MM |
INSIDE REINFORCEMENT | FIBERGLASS, STAINLESS STEEL, INCONEL |
.Chemical and Physical Data:
Chemical Composition (refractory fiber only):
Total Al2O3 and SiO2 >97% ( Al2O3: 47%); Fe2O3: < 1.1%
.Physical Properties:
Weight Loss(1800°F) 8-10%; Refractory fiber content > 85%
Fiber Diameter: 2 - 4 microns; Fiber Length: 100 - 250 mm
Fiber Shrinkage (1800°F, 3h): < 3.5%
Working Temperature : 1,800 °F. for Continuous Use; 2300 °F Maximum
.Thermal Conductivity:
570°F 0.84 BTU/sq.ft. °F/in (0.12 W/m °K)
1,100 °F 0.91 BTU/sq.ft. °F/in (0.13 W/m °K)
1,800 °F 1.19 BTU/sq.ft. °F/in (0.17 W/m °K)
Payment Terms: | T/T |
---|---|