the chemical composition of Kovar(%)
|
||||||||||
C
|
P
|
S
|
Mn
|
Si
|
Cu
|
Cr
|
Mo
|
Ni
|
Co
|
Fe
|
Not more than(≤)
|
|
|
|
|||||||
0.03
|
0.020
|
0.020
|
0.5
|
0.30
|
0.20
|
0.20
|
0.20
|
28.5~29.5
|
16.8~17.8
|
Balance
|
Status code
|
State
|
Tensile strength,N/mm2
|
R
1/4I
1/2I
3/4I
I
|
Soft state
1/4 Hard state
1/2 Hard state
3/4 Hard state
Hard state
|
<585
585—725
655—795
725—860
>860
|
Status code
|
State
|
Tensile strength,N/mm2
|
R
1/4I
1/2I
3/4I
I
|
Soft state
1/4 Hard state
1/2 Hard state
3/4 Hard state
Hard state
|
<570
520—630
590—700
600—770
>700
|
Alloy Grades
|
Specimen heat treatment system
|
The average linear expansion coefficienta,10-6/ oC
|
||
20-300 oC
|
20-400 oC
|
20-450 oC
|
||
kovar
|
In hydrogen atmosphere heated to 900 ± 20 oC, insulation lh, and then heated to 1100 ± 20 oC, insulation 15min, to not more than 5 oC / min rate of cooling to below 200 oC released
|
-----
|
4.6-5.2
|
5.1-5.5*
|
Alloy Grades
|
The average linear expansion coefficient a,10-6/ oC
|
|||||||
20-200
oC
|
20-300 oC
|
20-400
oC
|
20-450
oC
|
20-500
oC
|
20-600
oC
|
20-700
oC
|
20-800
oC
|
|
kovar
|
5.9
|
5.3
|
5.1
|
5.3
|
6.2
|
7.8
|
9.2
|
10.2
|