Product name :
Permanent magntes
The most powerful magnets available, Sintered NdFeB is produced by powder metallurgical process with chemical composition of Nd2Fe14B, which are hard, brittle and easily corrode, involving the sintering of compacts under vacuum. Poorest corrosion resistance of all commercial magnetic material. Grinding and slicing possible; very reactive with moisture and oxygen; coating may be applied depending on the expected environment. The sintered NdFeB magnet has high remanence, high coercive force, high-energy product and high ratio between performance value and product cost. It may be easily formed into various sizes. The intrinsic coercive force is over 30,000 Oe. Neodymium magnets lose -0.09 ~ -0.13% of Br/°C. Their working stability is under 80°C for low Hci. Neodymium magnets and above 200°C for high Hci Neodymium magnets. The highest (BH)max reaches up to 51MGOe . The choice of Strip casting and HDDR technology in our factory allows us to make high performance NdFeB over N52 possible. Surface treatments have been developed that allow the sintered NdFeB magnet to be used in most applications. The treatments include gold, nickel, zinc and tin plating and epoxy resin coating.
1. Materials:Neodymium-Iron-Boron;
2. Grades:N33-N52, 33M-48M, 33H-48H, 30SH-45SH, 30UH-38UH and 30EH-35EH;
3. Shapes and sizes: according to customers' request;
4. Coatings: Ni, Zn, gold, copper, epoxy, chemical, parylene and so on;.
5. Applications:sensors, motors, rotors, wind turbines/wind generators, loudspeakers, magnetic hooks, magnetic holder, filters automobiles and so on;
6. Utilizations of new Sintered NdFeB magnet techniques and equipment such as strip casting,HDDR technology;
7. High coercive force, the max operation temp is up to 200 degree centigrade or 380 curie temperature;
Magnetic Properties of Sintered NdFeB Magnets
|
Grade |
Remanence |
Coercivity Force |
Intrinsic Coercive Force |
Max. Energy Product |
maximum Operating Temp. |
Br |
Hcb |
Hcj |
( BH ) max |
mT |
kGs |
kA/m |
kOe |
kA/m |
kOe |
kJ/m3 |
MGOe |
N27 |
1030-1080 |
10.3-10.8 |
≥796 |
≥10.0 |
≥955 |
≥12 |
199-231 |
25-29 |
80 ℃ |
N30 |
1080-1130 |
10.8-11.3 |
≥796 |
≥10.0 |
≥955 |
≥12 |
223-247 |
28-31 |
80 ℃ |
N33 |
1130-1170 |
11.3-11.7 |
≥836 |
≥10.5 |
≥955 |
≥12 |
247-271 |
31-34 |
80 ℃ |
N35 |
1170-1220 |
11.7-12.2 |
≥868 |
≥10.9 |
≥955 |
≥12 |
263-287 |
33-36 |
80 ℃ |
N38 |
1220-1250 |
12.2-12.5 |
≥899 |
≥11.3 |
≥955 |
≥12 |
287-310 |
36-39 |
80 ℃ |
N40 |
1250-1280 |
12.5-12.8 |
≥907 |
≥11.4 |
≥955 |
≥12 |
302-326 |
38-41 |
80 ℃ |
N42 |
1280-1320 |
12.8-13.2 |
≥915 |
≥11.5 |
≥955 |
≥12 |
318-342 |
40-43 |
80 ℃ |
N45 |
1320-1380 |
13.2-13.8 |
≥923 |
≥11.6 |
≥955 |
≥12 |
342-366 |
43-46 |
80 ℃ |
N48 |
1380-1420 |
13.8-14.2 |
≥923 |
≥11.6 |
≥876 |
≥12 |
366-390 |
46-49 |
80 ℃ |
N50 |
1400-1450 |
14.0-14.5 |
≥796 |
≥10.0 |
≥876 |
≥11 |
382-406 |
48-51 |
60 ℃ |
N52 |
1430-1480 |
14.3-14.8 |
≥796 |
≥10.0 |
≥876 |
≥11 |
398-422 |
50-53 |
60 ℃ |
30M |
1080-1130 |
10.8-11.3 |
≥796 |
≥10.0 |
≥1114 |
≥14 |
223-247 |
28-31 |
100 ℃ |
33M |
1130-1170 |
11.3-11.7 |
≥836 |
≥10.5 |
≥1114 |
≥14 |
247-263 |
31-33 |
100 ℃ |
35M |
1170-1220 |
11.7-12.2 |
≥868 |
≥10.9 |
≥1114 |
≥14 |
263-287 |
33-36 |
100 ℃ |
38M |
1220-1250 |
12.2-12.5 |
≥899 |
≥11.3 |
≥1114 |
≥14 |
287-310 |
36-39 |
100 ℃ |
40M |
1250-1280 |
12.5-12.8 |
≥923 |
≥11.6 |
≥1114 |
≥14 |
302-326 |
38-41 |
100 ℃ |
42M |
1280-1320 |
12.8-13.2 |
≥955 |
≥12.0 |
≥1114 |
≥14 |
318-342 |
40-43 |
100 ℃ |
45M |
1320-1380 |
13.2-13.8 |
≥995 |
≥12.5 |
≥1114 |
≥14 |
342-366 |
43-46 |
100 ℃ |
48M |
1360-1430 |
13.6-14.3 |
≥1027 |
≥12.9 |
≥1114 |
≥14 |
366-390 |
46-49 |
100 ℃ |
50M |
1400-1450 |
14.0-14.5 |
≥1033 |
≥13.0 |
≥1114 |
≥14 |
382-406 |
48-51 |
100 ℃ |
30H |
1080-1130 |
10.8-11.3 |
≥796 |
≥10.0 |
≥1353 |
≥17 |
223-247 |
28-31 |
120 ℃ |
33H |
1130-1170 |
11.3-11.7 |
≥836 |
≥10.5 |
≥1353 |
≥17 |
247-271 |
31-34 |
120 ℃ |
35H |
1170-1220 |
11.7-12.2 |
≥868 |
≥10.9 |
≥1353 |
≥17 |
263-287 |
33-36 |
120 ℃ |
38H |
1220-1250 |
12.2-12.5 |
≥899 |
≥11.3 |
≥1353 |
≥17 |
287-310 |
36-39 |
120 ℃ |
40H |
1250-1280 |
12.5-12.8 |
≥923 |
≥11.6 |
≥1353 |
≥17 |
302-326 |
38-41 |
120 ℃ |
42H |
1280-1320 |
12.8-13.2 |
≥955 |
≥12.0 |
≥1353 |
≥17 |
318-342 |
40-43 |
120 ℃ |
45H |
1300-1360 |
13-13.6 |
≥963 |
≥12.1 |
≥1353 |
≥17 |
326-358 |
43-46 |
120 ℃ |
48H |
1370-1430 |
13.7-14.3 |
≥995 |
≥12.5 |
≥1353 |
≥17 |
366-390 |
46-49 |
120 ℃ |
30SH |
1080-1130 |
10.8-11.3 |
≥804 |
≥10.1 |
≥1592 |
≥20 |
223-247 |
28-31 |
150 ℃ |
33SH |
1130-1170 |
11.3-11.7 |
≥844 |
≥10.6 |
≥1592 |
≥20 |
247-271 |
31-34 |
150 ℃ |
35SH |
1170-1220 |
11.7-12.2 |
≥876 |
≥11.0 |
≥1592 |
≥20 |
263-287 |
33-36 |
150 ℃ |
38SH |
1220-1250 |
12.2-12.5 |
≥907 |
≥11.4 |
≥1592 |
≥20 |
287-310 |
36-39 |
150 ℃ |
40SH |
1240-1280 |
12.5-12.8 |
≥939 |
≥11.8 |
≥1592 |
≥20 |
302-326 |
38-41 |
150 ℃ |
42SH |
1280-1320 |
12.8-13.2 |
≥987 |
≥12.4 |
≥1592 |
≥20 |
318-342 |
40-43 |
150 ℃ |
45SH |
1320-1380 |
13.2-13.8 |
≥1003 |
≥12.6 |
≥1592 |
≥20 |
342-366 |
43-46 |
150 ℃ |
28UH |
1020-1080 |
10.2-10.8 |
≥764 |
≥9.6 |
≥1990 |
≥25 |
207-231 |
26-29 |
180 ℃ |
30UH |
1080-1130 |
10.8-11.3 |
≥812 |
≥10.2 |
≥1990 |
≥25 |
223-247 |
28-31 |
180 ℃ |
33UH |
1130-1170 |
11.3-11.7 |
≥852 |
≥10.7 |
≥1990 |
≥25 |
247-271 |
31-34 |
180 ℃ |
35UH |
1180-1220 |
11.8-12.2 |
≥860 |
≥10.8 |
≥1990 |
≥25 |
263-287 |
33-36 |
180 ℃ |
38UH |
1220-1250 |
12.2-12.5 |
≥876 |
≥11.0 |
≥1990 |
≥25 |
287-310 |
36-39 |
180 ℃ |
40UH |
1240-1280 |
12.5-12.8 |
≥899 |
≥11.3 |
≥1990 |
≥25 |
302-326 |
38-41 |
180 ℃ |
28EH |
1040-1090 |
10.4-10.9 |
≥780 |
≥9.8 |
≥2388 |
≥30 |
207-231 |
26-29 |
200 ℃ |
30EH |
1080-1130 |
10.8-11.3 |
≥812 |
≥10.2 |
≥2388 |
≥30 |
223-247 |
28-31 |
200 ℃ |
33EH |
1130-1170 |
11.3-11.7 |
≥836 |
≥10.5 |
≥2388 |
≥30 |
247-271 |
31-34 |
200 ℃ |
35EH |
1170-1220 |
11.7-12.2 |
≥876 |
≥11.0 |
≥2388 |
≥30 |
263-287 |
33-36 |
200 ℃ |
38EH |
1220-1250 |
12.2-12.5 |
≥899 |
≥11.3 |
≥2388 |
≥30 |
287-310 |
36-39 |
200 ℃ |
|
|
Physical Properties of Sintered NdFeB Magnets |
Temp.Coeff.of Br |
-0.11%/ ℃ |
Temp.Coeff.of Hc |
-0.60%/ ℃ |
Density |
7.3-7.5g/cm 3 |
Electrical Resistivity |
114 μΩ ..cm |
Vickers Hardness |
600Hv |
Flexural Resistivity |
25kg/mm |
Tensile Strength |
8.0Kg/mm2 |
Coeff. Of Thermal Expansion |
4X10 -6 / ℃ |
Specific Heat |
0.12Kcal/Kg |
Thermal Conductivity |
7.7kcal/[m.h. ℃ ] |
Young's Modulus |
1.6X10[11]N/m2 |
Rigidity |
0.64N/m2 |
Poisson's Ratio |
0.24 |
Compressibility |
9.8x10-12m2/N |
Curie Temperature |
310-340 ℃ |
|
|
|
|
sintered NdFeB magnet has been presented above, want more similar products, please click NdFeB magnets,rare earth permanent magnets,sintered neodymium magnet.
Our sintered NdFeB magnet is good in quality and competitive in price. We manufacture sintered NdFeB magnet and supply OEM, ODM service according to your requirement.
If you want more detailed information of this product or related problems, please contact with us, we will reply as soon as possible (general in 24 hours).