304 stainless steel screen
The ultimate tensile strength of B (MPa) = 520
Atlas of 304 stainless steel
304 stainless steel Atlas (7)
Conditional yield strength (MPa = 205) 0.2
5 elongation (%) = 40
Section shrinkage (%) = 60 PSI
Hardness: = 187HB; 90HRB = 200HV;
Density (20 DEG C, g/cm3): 7.93
Melting point (c): 1398~1454
The specific heat (C 0~100, KJ, kg-1K-1): 0.50
Thermal conductivity (W. M-1. K-1): (100 DEG C), 16.3, (C = C), 21.5
Coefficient of linear expansion (10-6 = K-1): (0~100 DEG C) 17.2, (0~500 DEG C), 18.4
Resistivity (20, 10-6) (m)
Longitudinal modulus of elasticity (20 DEG C, KN/mm2): 193