Product Description

Name
 
High temperature resistant fiber glass adhesivesTHO4057
Outline
It is double-component epoxy adhesive. It is easy and convenient to use for it solidifies fast at normal temperature and bonds well.
Applications
This product is widely applied to the coating, bonding, sealing, filling, repairing of fiber glass made from silicate, blended fabric composite materials and other materials. 
Features
The A component is the tinted thick liquid, non-solid particle. The B component is in tinted paste shape. 
Fast curing speed. At 25°C 1-3 hour it is at the early stage of curing, 18 hours later, it reaches its maximum bonding strength. 
It cures during 40-60 minutes if put into heating oven of 80-100  
Being durable and resistant to ultraviolet light, once the bond has formed.
Being heat-resistant, it adapts to a wide range of temperature and bonds well under high temperature. 
With moderate viscosity, the adhesive leaves no bubbles, making the surface smooth and bright.
Mix the two components in a certain proportion, apply it to the surface of the substrates directly, which makes it so convenient to use. 

You'll get long term durability and resistance to moisture, chemicals, oils, and temperature extremes.

 
Non-toxic after solidification, though it is a little smelly.
 
Being stable, its shelf life is one and a half year.
The main technical parameters are as follows:

Heat resistance scope-40°C+400°C

 
Cementation intensity:   Normal temperature:
Tensile strength25MPa; Shearing strength20 MPa
150℃: Tensile strength  3-5 MPa
Instruction
 
1. Clean the surface of the material, make sure they have no dust or oil on them, wait until they are dry.
2. Mix A and B in a proportion of 10: 1.2--1.5 to get perfect bonding result at fastest speed at 25°C.
3. Spread the mixture on the substrates, put them together and apply some strength on them, finally, let them dry for 2-4 hours.
4. If the surface of ceramics needs to be shaped after the coating, hot press molding or cold press molding should be applied when the adhesive is in its preliminary curing time.
Notes
1. Use another can or container to blend A with B. The tools used to get A and B should be different.
2. A and B should be mixed well.

3. It is necessary to keep it well ventilated and away from fire.

 
4. If it has contact with skin, you should wash thoroughly with soap and water.
 

5. It can be stored at well-ventilated places with low temperature, and keep them away from fire.

 
6. Cover the lip after using it.
   Copyright © 2005-2010Thomas Technology, Inc. All Rights Reserved.
 
Thomas high temperature resistant fiberglass adhesive 1

Member Information

Thomas Sci Co.,Ltd
Country/Region:Si chuan - China
Business Nature:Manufacturer
Phone:13348852062
Contact:Makeda (manager)
Last Online:11 Jun, 2015