Packing specification of BD706 large particle anti wear corrosion resistant coatings:
Two component,10Kg/group,packed in a plastic drum
performance feature of BD706 anti corrosive abrasion resistant large particle coating:
dark gray paste,large particle,room temperature curing
Excellent in wear & corrosion resistance
BD706 Abrasion Resistant coatings and the metal substrate with high bonding strength
Convenient for construction,without very high technical requirements for constructors
Suitable for the repairing and protecting of various wear,corrosion working condition
product usage of BD706 large particle anti abrasive corrosive resistant adhesive:
It is the high performance wear & corrosion resistant polymerization ceramic material compounded by high performance wear resistant ceramic particles and modified toughening resin.Widely used in the repairing of various wear-out parts and the preparation of wear & corrosion resistant coating on the surface of various machine part which has wear resistant,corrosion resistant requirements,such as the repairing and pre-protecting of large load fine particle erosive wear pump body,impeller,fan shell,pipeline elbow,pipeline spiral conveyor etc.
How to use of anti corrosion abrasion resistant large particle adhesives:
1. Surface treatment:Do coarsening treatment on the pending-repair part,grinding with angle grinder or sand blasting etc,the surface after coarsening treatment should be cleaned,the surface after this treatment should be the one coarsening,dry and fresh substrates,should be no greasy dirt and dust.
2. Preparation:According to weight ratio or volume ratio 4:1,make A and B two components mix uniformly,and use it up within 30 min.Generally it’s while construction and configuration.Every time the most configuration quantity is not more than 1.5Kg,too much adhesive is solidified too fast,hasn’t been used up until the adhesive has partial solidified and can’t be used.According to the actual temperature,configuration can be properly a little more in winter and proper less in summer.If the temperature is too low,can properly heat up the A component to reduce viscosity for easy to configure.